Cube mould inside faces must be machined plane. cube mould is normally made in two halves to facilitate removal of the concrete cube without damage. Each mould has a base, which is a separate metal plate, preferably fastened to the mold by clamps or springs. When assembled, all the internal angles of the mold must be right angles. Distance between opposite faces, mm (150 ± 0.2), Height of mould, mm(150 ± 0.2), Thickness of wall plate, mm(8), materials Side plate & Base plate- Cast iron, Angle between adjacent interior faces and between interior faces and top and bottom plates of mold. 90 ± 0.50.